VORON 1.5: Bad first layer scaring
- by Tom Beyer
- 2017-03-13
- 3D Printing
I made my first big print on my new VORON this weekend. After adjusting the level of the bed with my dial indicator I'am pretty happy with the general "flatness/adhesion" with my first layer.
Unfortunately i get really bad "scars" in the middle of the layer which makes strange patterns. Currently i have no idea whats wrong here.
Used settings
Nozzle: 0.6mm
Layer height: 0.4mm
Print speed: 60mm/sec
First layer height: 50%
First layer print speed: 50%
Z-Offset 1.5mm
Black HERZ PLA
Temperature First layer: 205°C
Fan off